类别
Type
|
牌号
Grade
|
合金成分
Alloy
Components
|
物理-机械性能
Physical Mechanism Characteristics
|
主要应用
Application
|
|
密度
Density
(g/cm3)
|
含油率
|
压溃强度
|
表现硬度
Apparent
Hardness
(HB)
|
|
铁基
Iron
Base
|
FZ1260
|
Fe-C
|
5.7~6.2
|
≥18
|
>25
|
50~100
|
风扇,洗衣机搅
拌机等电配件,
办公设备仪表等
Electric Fan,
Washing Machine,
Mixer,Household
Appliance part;
Office Facilities
And Meter,ETC.
|
|
FZ1265
|
Fe-C
|
6.2~6.6
|
≥12
|
>30
|
60~110
|
|
FZ1360
|
Fe-C-Cu
|
5.7~6.3
|
≥18
|
>35
|
60~110
|
|
FZ1365
|
Fe-C-Cu
|
6.2~6.6
|
≥12
|
>40
|
70~120
|
|
AFZ1460
|
Fe-Cu
|
5.8~6.3
|
≥18
|
>28
|
50~100
|
|
BFZ1460
|
Fe-Cu
|
5.8~6.3
|
≥18
|
>15
|
40~70
|
|
铜基
Copper
Base
|
FZ2170
|
Cu-Sn-Zn-Pb
|
6.6~7.2
|
≥18
|
>15
|
20~50
|
|
FZ2175
|
Cu-Sn-Zn-Pb
|
7.2~7.8
|
≥12
|
>20
|
30~60
|
高精度、低噪音、耐高速微型含油轴承
High
Accacy、Low Noise、Lasting High Speed Running Micro Oil
Impregated Bearing
|
材料
Type
|
物理-机械性能
|
|
密度
Density
g/cm3
|
噪音
Noise
(距离50mm),
dB
|
含油率
Oil
Contained
(容积)%
|
磨损量
Wear Extent
μm
|
摩擦系数
|
压溃
强度
|
表面硬度
Apparent
Hardness(300g/30s)
MHv
|
寿命
Life_time
(3000rpm
×500g),h
|
|
铜基
Copper
Base
|
6.5~7.5
|
< 20
|
> 18
|
< 12
|
< 0.4
|
> 216
|
60~90
|
> 2000
|
|
铁铜基
Iron And
Copper
Base
|
6.0~6.8
|
< 20
|
> 18
|
< 12
|
< 0.25
|
> 216
|
60~100
|
> 2000
|
|
铁基
Iron
Base
|
5.9~6.6
|
< 20
|
> 18
|
< 12
|
< 0.30
|
> 245
|
60~100
|
> 2000
|
铁基结构材料 Iron
Base Components
|
类 别
Type
|
合金成分
Alloy
Components
|
物理-机械性能
Physical Mechanism
Characteristics
|
主要应用
|
|
抗拉强度
|
延伸率
|
冲击韧性
|
密度
Density
(g/cm3)
|
表观硬度
Apparent
Hardness
(HB)
|
|
烧结铁
Sintered Iron
|
Fe-C
|
≥10
|
≥3.0
|
≥0.5
|
6.2~7.0
|
≥40
|
摩托车,汽车
电动工具,家
用电器等
Motor Bike,
Vehicle,
Electric Tools,
Household
Appliance,ETC
|
|
烧结低碳钢
Sintered Low
carbon steel
|
Fe-C
|
≥10
|
≥1.5
|
≥0.5
|
6.2~7.0
|
≥50
|
|
烧结中碳钢
Sintered Medium
Carbon Steel
|
Fe-C
|
≥15
|
≥1.0
|
≥0.5
|
6.2~7.0
|
≥60
|
|
烧结高碳钢
Sintered High
Carbon Steel
|
Fe-C
|
≥20
|
≥0.5
|
≥0.3
|
6.2~7.0
|
≥70
|
|
烧结铜钢
Sintered
Copper Steel
|
Fe-C-Cu
|
≥25
|
≥0.5
|
≥0.3
|
6.2~7.0
|
≥90
|
|